Superalloy Waspaloy sheet, Waspaloy 25 strip price, Waspaloy plate, Waspaloy round bar manufacture
1.Rod, Bar, Wire and Forging Stock
2.ASTM B 637, ISO 9723, ISO 9724, ISO 9725, AMS 5704, AMS 5706, AMS 5707, AMS 5708, AMS 5709, AMS 5828, MAM 5706, AECMA PrEN 2193, AECMA PrEN 2194, AECMA PrEN 2406, AECMA PrEN 2958, AECMA PrEN 2959, AECMA PrEN 2960, AECMA PrEN 3220.
3.Plate, Sheet and Strip
4.AMS 5544, AECMA PrEN 2195
5.Other
6.UNS N07001, W. Nr 2.4654, MSRR 7192
Properties as per AMS 5708 type 2 (capable of AMS 5709) Heat Treatment is as follows
Solution Treat 1900 - 1975°F / 1-4 hours and Air Cool
Resulting hardness not higher than 302HB
Stabilization Heat Treatment Heat to 1550°F / 4 hrs and Air Cool
Precipitation Heat Treatment Heat to 1400°F / 16 hrs and Air Cool
Resulting hardness 32-42 HRC
Heat Treatment is as follows
Annealing 1975°F / 30 mins and Air Cool
Solution Heat Treatment 1825°F / 2hrs and Air Cool
Stabilization Heat Treatment 1550°F /4hrs and Air Cool
Precipitation Heat Treatment 1400°F / 16 hrs and Air Cool
| Cr | 18.0-21.0 | B | 0.003-0.01 |
| Zr | 0.02-0.12 | Al | 1.2-1.6 |
| Ti | 2.75-3.25 | Mo | 3.5-5.0 |
| Co | 12.0-15.0 | Cu | 0.5 max |
| Fe | 2.0 max | S | 0.03 max |
| Si | 0.75 max | Mn | 1.0 max |
| C | 0.02-0.1 max | P | 0.03 max |
| Ni | Balance |
| Material | Condition | Thickness | Temp. | Tensile Strength ksi | Yield Strength ksi | Elongation in 4D | Hardness HRC |
| Sheet | Sol Treated, Stabilization + Precipitation HT | 0-0.020" | Room | 170 | 110 | 15 | 34-44 |
| Sheet | Sol Treated, Stabilization + Precipitation HT | 0-0.020" | 1000°F | 145 | 100 | 13 | |
| Sheet | Sol Treated, Stabilization + Precipitation HT | over 0.020" | Room | 175 | 115 | 20 | 34-44 |
| Sheet | Sol Treated, Stabilization + Precipitation HT | over 0.020" | 1000°F | 150 | 105 | 15 |